Skip to main content

Besmak

LONG TERM CREEP TESTING MACHINE – BMT-C

BESMAK Long Term Creep Testing Machine is designed for precise long-duration creep and stress-rupture testing of concrete, metals, composites, and other engineering materials. The servo hydraulic system applies and maintains constant loads for hours, days, months, or even years, enabling highly accurate measurement of time-dependent deformation under controlled laboratory conditions.

Servo Hydraulic Long Term Creep Testing Equipment

The BESMAK Long Term Creep Testing Machine uses an advanced servo hydraulic loading system combined with mechanical spring-assisted load maintenance. This design ensures stable and uninterrupted long-term loading while minimizing energy consumption and operator intervention. The system is ideal for research laboratories, universities, and industrial quality control applications.

 

Key Features of the Long Term Creep Testing Machine

Servo Hydraulic Load Control

Provides precise and fully automatic load application with closed-loop control.

 

Long-Term Constant Load Maintenance

Maintains stable test loads for extended periods ranging from several hours to multiple years.

 

Mechanical Spring-Assisted Loading

Reduces continuous hydraulic pump operation and improves energy efficiency.

 

Multi-Specimen Testing Capability

Tests up to three specimens simultaneously using one loading frame.

 

Zero-Drift Deformation Sensors

Ensures accurate long-term strain and displacement measurements.

 

Advanced Creep Test Software

Supports both short-term and long-term creep test protocols with automatic data recording.

 

Automated Data Analysis

Provides extrapolation and interpretation of long-term material behavior.

 

Ergonomic User Interface

Offers intuitive controls for easy setup and monitoring.

 

Modular Architecture

Allows integration of additional sensors and custom test procedures.

 

 

Main Components of the Long Term Creep Testing Machine

 

Universal Testing Software

Controls test parameters, data acquisition, and automated reporting.

 

Four-Column Loading Frame

High-rigidity frame with servo hydraulic actuator and mechanical springs.

 

Creep Test Frame

150 × 300 mm specimen configuration with simultaneous multi-sample testing.

 

Load Measurement System

High-accuracy load cells with EN ISO 7500-1 Class 1 or better performance.

 

Hydraulic Power Unit

Fast-response servo hydraulic system with multi-piston pump and precision valves.

 

 

Applications of the Long Term Creep Testing Machine

 

Concrete Creep Testing

Compression Creep Testing

Stress-Rupture Testing

Metal Creep Testing

Composite Material Creep Testing

Polymer and Plastic Creep Testing

University and Research Applications

 

 

Technical Specifications

Available Capacities

  • 300 kN, 500 kN, 600 kN, and 1000 kN

 

Specimen Size

150 × 300 mm standard concrete cylinders

 

Number of Specimens

Up to 3 specimens tested simultaneously

 

Control Type

Fully automatic servo hydraulic closed-loop control

 

Measurement Sensors

Load cells, displacement transducers, and compression sensors

 

Software Functions

Real-time monitoring, automated reporting, and long-term analysis

 

Available Models

BMT-300STC – Long Term Creep Testing Machine, 300 kN Capacity

BMT-500STC – Long Term Creep Testing Machine, 500 kN Capacity

BMT-600STC – Long Term Creep Testing Machine, 600 kN Capacity

BMT-1000STC – Long Term Creep Testing Machine, 1000 kN Capacity

 

 

Benefits for Research Laboratories and Material Testing Centers

Accurate Long-Term Deformation Measurement

Stable Constant Load Application

Reduced Energy Consumption

Simultaneous Multi-Specimen Testing

Automated Data Collection and Reporting

Compliance with International Standards

 

 

Supported Standards

ASTM C512

ISO 1920

EN Standards for Creep Testing

Other National and International Standards

 

Why Choose BESMAK?

30+ Years of Engineering Experience

BESMAK has been manufacturing advanced material testing systems for more than 30 years.

 

Export to 75+ Countries

Our equipment is trusted by laboratories, universities, and manufacturers worldwide.

 

Customized Long-Term Testing Solutions

Systems can be tailored to specific specimen sizes, capacities, and research requirements.

 

Global Technical Support

Comprehensive installation, training, and after-sales service.

 

Frequently Asked Questions

What is a Long Term Creep Testing Machine?

A testing system used to measure time-dependent deformation under constant load over extended periods.

 

Which materials can be tested?

Concrete, metals, composites, polymers, and other engineering materials.

 

How long can the tests run?

From a few hours to several years, depending on the application.

 

How many specimens can be tested simultaneously?

Up to three specimens can be tested in one frame.

 

Which standards are supported?

ASTM C512, ISO 1920, and other international creep testing standards.

 

 

Request a Quote for Long Term Creep Testing Machine

Contact BESMAK today to receive technical specifications, pricing, and customized solutions for long-term creep and stress-rupture testing applications.

 

Product Code Product Name
BMT-300STC Servo Hydraulic Creep Test Machine 300 kN Capacity
BMT-500STC Servo Hydraulic Creep Test Machine 500 kN Capacity
BMT-600STC Servo Hydraulic Creep Test Machine 600 kN Capacity
BMT-1000STC Servo Hydraulic Creep Test Machine 1000 kN Capacity